Highly Tunable Nanostructures in a Doubly pH‐Responsive Pentablock Terpolymer in Solution and in Thin Films

Jung F, Schart M, Bührend L, Meidinger E, Kang J, Niebuur B, Ariaee S, Molodenskiy D, Posselt D, Amenitsch H, Tsitsilianis C, Papadakis C
Advanced Functional Materials 31(32):2102905 (2021 Jun 03)

doi: 10.1002/adfm.202102905
Submitted to SASBDB: 2021 May 10
Published in SASBDB:

SASDPG8 – Solution of 0.1 wt% pentablock terpolymer (M18D170V209D170M18) in water at pH 2.6

M18D170V209D170M18 experimental SAS data
M18D170V209D170M18 Kratky plot
Sample: M18D170V209D170M18 monomer, 1 kDa
Buffer: H20, pH: 2.6
Experiment: SAXS data collected at EMBL P12, PETRA III on 2020 Dec 5
RgGuinier 8.7 nm

SASDPH8 – Solution of 0.1 wt% pentablock terpolymer (M18D170V209D170M18) in water at pH 5.0

M18D170V209D170M18 experimental SAS data
M18D170V209D170M18 Kratky plot
Sample: M18D170V209D170M18 monomer, 1 kDa
Buffer: H2O, pH: 5
Experiment: SAXS data collected at EMBL P12, PETRA III on 2020 Dec 5
RgGuinier 8.2 nm

SASDPJ8 – Solution of 0.1 wt% pentablock terpolymer (M18D170V209D170M18) in water at pH 6.9

M18D170V209D170M18 experimental SAS data
M18D170V209D170M18 Kratky plot
Sample: M18D170V209D170M18 monomer, 1 kDa
Buffer: H2O, pH: 6.9
Experiment: SAXS data collected at EMBL P12, PETRA III on 2020 Dec 5
RgGuinier 5.4 nm

SASDPK8 – Solution of 0.1 wt% pentablock terpolymer (M18D170V209D170M18) in water at pH 8.9

M18D170V209D170M18 experimental SAS data
M18D170V209D170M18 Kratky plot
Sample: M18D170V209D170M18 monomer, 1 kDa
Buffer: H2O, pH: 8.9
Experiment: SAXS data collected at EMBL P12, PETRA III on 2020 Dec 5
RgGuinier 7.3 nm